LBG-32 BELT SURFACE GRINDING SPECIMEN MACHINE

Model

LBG-32

Distance between the centers of two rollers

274mm

Cooling method

water cooling and dust separation plant

Power supply

380V, 50Hz

Surface speed

768 m / min

Rotating speed

1400 rpm

Grinding size

220 x 120mm

Sand belt

1003 x 100mm (L x W)

Motor

750W

Dimension

580 x 600 x 980 mm


BG-30 BELT SURFACE GRINDING SPECIMEN MACHINE

Model

BG-30

Distance between the centers of two rollers

255mm

Cooling method

water cooling

Power supply

three phases, 380V, 50Hz

Surface speed

768 m / min

Rotating speed

1400 rpm

Sand belt

920mm x 100mm (L x W)

Motor

550W


BG-32 Metallographic Sample Coarse Grinder

Distance between roller''s center:274mm

water cooling system and dust separation plant

Belt:100mm width 1003 length

Rotation:1400rpm

Surface speed:768rpm

Motor:750W

Power:380V/50HZ

Dimension:580*600*980mm

Grinding Size:220*120mm